4. All zinc deposits and polished parts need to be repainted with cold galvanized layer, and the minimum average thickness of the zinc layer is 19.3μm.
4. All zinc deposition polishing areas need to be repainted with a cold galvanized layer, with a minimum average thickness of 19.3 for the zinc layer μ m。