The defect rate of scratches in the post production process of steel sheets was investigated by the station, and the defect rate of scratches was found to be 2.5%, accounting for 75%, after cutting the inner groove
After the by station of steel sheet post-process inspection, the by process inspection showed that the scratch defect was increased by 2.5%, accounting for 75%.