Product Name: 800007_LNRoot Cause Analysis: 1. There were +/- 0.25 inch tolerance for these bags. And the cutting width during Lamination was fixed. The side of the larger bag was cut during the lamination process, causing the bags to be broken. 2. During the inspection process, staff did not pick all of the defect bags out. Corrective Action and Preventive Action Plan: 1. Lamination Side-Cutting machine has been changed from manual control to ultrasonic tracking device. The bags in process should not have such problem anymore. 2. Skilled & careful workers are pointed to pick the detect bags out. We will also develop QC performance assessment program and make sure no detect bags pass through inspection. Please tell us how many bags are unused so we can figure out a return & compensation plan.